6YA7
Cdc7-Dbf4 bound to an Mcm2-S40 derived bivalent substrate
Experimental procedure
Experimental method | SINGLE WAVELENGTH |
Source type | SYNCHROTRON |
Source details | DIAMOND BEAMLINE I03 |
Synchrotron site | Diamond |
Beamline | I03 |
Temperature [K] | 100 |
Detector technology | PIXEL |
Collection date | 2014-04-19 |
Detector | DECTRIS PILATUS3 6M |
Wavelength(s) | 0.97625 |
Spacegroup name | P 41 21 2 |
Unit cell lengths | 62.280, 62.280, 234.790 |
Unit cell angles | 90.00, 90.00, 90.00 |
Refinement procedure
Resolution | 60.200 - 1.670 |
R-factor | 0.1577 |
Rwork | 0.156 |
R-free | 0.18520 |
Structure solution method | MOLECULAR REPLACEMENT |
Starting model (for MR) | 5MH9 |
RMSD bond length | 0.010 |
RMSD bond angle | 1.151 |
Data reduction software | XDS |
Data scaling software | Aimless |
Phasing software | PHASER |
Refinement software | PHENIX (dev_3707) |
Data quality characteristics
Overall | Outer shell | |
Low resolution limit [Å] | 60.200 | 1.710 |
High resolution limit [Å] | 1.670 | 1.670 |
Rmerge | 0.098 | 0.724 |
Number of reflections | 54941 | 5401 |
<I/σ(I)> | 19.4 | |
Completeness [%] | 100.0 | |
Redundancy | 12.5 | |
CC(1/2) | 1.000 | 0.810 |
Crystallization Conditions
crystal ID | method | pH | temperature | details |
1 | VAPOR DIFFUSION, HANGING DROP | 7 | 291.15 | 0.1M PCTP pH7, 18% PEG 1500, 8% MPD |