8ZR2
Cocrystallization of engineered streptavidin with C9 oligo DNA
Experimental procedure
Experimental method | SINGLE WAVELENGTH |
Source type | SYNCHROTRON |
Source details | PHOTON FACTORY BEAMLINE AR-NW12A |
Synchrotron site | Photon Factory |
Beamline | AR-NW12A |
Temperature [K] | 100 |
Detector technology | CCD |
Collection date | 2015-12-08 |
Detector | ADSC QUANTUM 270 |
Wavelength(s) | 1.000 |
Spacegroup name | C 1 2 1 |
Unit cell lengths | 80.937, 80.986, 77.316 |
Unit cell angles | 90.00, 91.97, 90.00 |
Refinement procedure
Resolution | 46.540 - 2.500 |
R-factor | 0.2399 |
Rwork | 0.234 |
R-free | 0.34560 |
Structure solution method | MOLECULAR REPLACEMENT |
Starting model (for MR) | 6lng |
RMSD bond length | 0.008 |
RMSD bond angle | 1.144 |
Data reduction software | XDS |
Data scaling software | XSCALE |
Phasing software | PHENIX |
Refinement software | PHENIX (1.9_1692) |
Data quality characteristics
Overall | Outer shell | |
Low resolution limit [Å] | 46.540 | 2.560 |
High resolution limit [Å] | 2.500 | 2.500 |
Rmerge | 0.165 | 0.889 |
Number of reflections | 17327 | 1265 |
<I/σ(I)> | 7.63 | 1.9 |
Completeness [%] | 99.8 | 99.4 |
Redundancy | 3.7 | 3.6 |
CC(1/2) | 0.989 | 0.633 |
Crystallization Conditions
crystal ID | method | pH | temperature | details |
1 | BATCH MODE | 8 | 298 | 20 mM Tris-HCl |