7Z3W
Crystal structure of the AAL160 Fab
Experimental procedure
Experimental method | SINGLE WAVELENGTH |
Source type | SYNCHROTRON |
Source details | ESRF BEAMLINE BM02 |
Synchrotron site | ESRF |
Beamline | BM02 |
Temperature [K] | 100 |
Detector technology | IMAGE PLATE |
Collection date | 1999-06-18 |
Detector | MAR scanner 300 mm plate |
Wavelength(s) | 0.7998 |
Spacegroup name | P 21 21 21 |
Unit cell lengths | 62.173, 89.832, 123.734 |
Unit cell angles | 90.00, 90.00, 90.00 |
Refinement procedure
Resolution | 16.380 - 2.000 |
R-factor | 0.1979 |
Rwork | 0.196 |
R-free | 0.21750 |
Structure solution method | MOLECULAR REPLACEMENT |
Starting model (for MR) | 1MIM.PDB |
RMSD bond length | 0.008 |
RMSD bond angle | 1.010 |
Data reduction software | HKL-2000 (1.96.1) |
Data scaling software | SCALEPACK (1.96.1) |
Phasing software | AMoRE (3.4) |
Refinement software | BUSTER (2.11.8) |
Data quality characteristics
Overall | Inner shell | Outer shell | |
Low resolution limit [Å] | 28.000 | 28.000 | 2.070 |
High resolution limit [Å] | 2.000 | 4.300 | 2.000 |
Rmerge | 0.050 | 0.033 | 0.381 |
Number of reflections | 47440 | 5003 | 4670 |
<I/σ(I)> | 11.7 | ||
Completeness [%] | 99.9 | 99.7 | 100 |
Redundancy | 8.34 |
Crystallization Conditions
crystal ID | method | pH | temperature | details |
1 | VAPOR DIFFUSION, HANGING DROP | 9.5 | 293 | 0.1M CHES pH 9.5, 50% (w/v) PEG 200 |