6Z8Y
Copper transporter OprC
Experimental procedure
| Experimental method | SINGLE WAVELENGTH |
| Source type | SYNCHROTRON |
| Source details | DIAMOND BEAMLINE I24 |
| Synchrotron site | Diamond |
| Beamline | I24 |
| Temperature [K] | 100 |
| Detector technology | PIXEL |
| Collection date | 2019-11-23 |
| Detector | DECTRIS PILATUS3 6M |
| Wavelength(s) | 1.40889 |
| Spacegroup name | P 2 21 21 |
| Unit cell lengths | 67.032, 170.742, 198.043 |
| Unit cell angles | 90.00, 90.00, 90.00 |
Refinement procedure
| Resolution | 67.030 - 2.780 |
| R-factor | 0.2131 |
| Rwork | 0.210 |
| R-free | 0.26620 |
| Structure solution method | MOLECULAR REPLACEMENT |
| Starting model (for MR) | 6fok |
| RMSD bond length | 0.009 |
| RMSD bond angle | 1.116 |
| Data reduction software | xia2 |
| Data scaling software | Aimless |
| Phasing software | PHENIX |
| Refinement software | PHENIX (1.17.1_3660) |
Data quality characteristics
| Overall | Outer shell | |
| Low resolution limit [Å] | 198.040 | 2.830 |
| High resolution limit [Å] | 2.780 | 2.780 |
| Rpim | 0.078 | |
| Number of reflections | 58146 | 5698 |
| <I/σ(I)> | 5.52 | |
| Completeness [%] | 100.0 | |
| Redundancy | 12.66 | |
| CC(1/2) | 0.400 |
Crystallization Conditions
| crystal ID | method | pH | temperature | details |
| 1 | VAPOR DIFFUSION, HANGING DROP | 5.5 | 293 | 0.34 M Ammonium sulfate 0.1 M Sodium citrate 12 -16 % w/v PEG 4000 |