5OYZ
Automated refinement of diffraction data obtained from an endothiapepsin crystal treated with fragment 10
Experimental procedure
| Experimental method | SINGLE WAVELENGTH |
| Source type | SYNCHROTRON |
| Source details | BESSY BEAMLINE 14.1 |
| Synchrotron site | BESSY |
| Beamline | 14.1 |
| Temperature [K] | 100 |
| Detector technology | CCD |
| Collection date | 2012-09-04 |
| Detector | MARMOSAIC 225 mm CCD |
| Wavelength(s) | 0.91841 |
| Spacegroup name | P 1 21 1 |
| Unit cell lengths | 45.277, 72.431, 52.430 |
| Unit cell angles | 90.00, 108.65, 90.00 |
Refinement procedure
| Resolution | 36.911 - 1.487 |
| R-factor | 0.1294 |
| Rwork | 0.128 |
| R-free | 0.15540 |
| Structure solution method | MOLECULAR REPLACEMENT |
| Starting model (for MR) | 4y5l |
| RMSD bond length | 0.008 |
| RMSD bond angle | 1.203 |
| Data reduction software | XDS |
| Data scaling software | XDS |
| Phasing software | PHASER (2.5.7) |
| Refinement software | PHENIX |
Data quality characteristics
| Overall | Inner shell | Outer shell | |
| Low resolution limit [Å] | 42.899 | 1.580 | |
| High resolution limit [Å] | 1.490 | 4.440 | 1.490 |
| Rmerge | 0.048 | 0.017 | 0.384 |
| Rmeas | 0.055 | 0.020 | 0.444 |
| Total number of observations | 216433 | ||
| Number of reflections | 52380 | 2022 | 8190 |
| <I/σ(I)> | 20.59 | 56.37 | 3.66 |
| Completeness [%] | 99.3 | 99.1 | 96.4 |
| Redundancy | 4.131 | ||
| CC(1/2) | 0.999 | 1.000 | 0.877 |
Crystallization Conditions
| crystal ID | method | pH | temperature | details |
| 1 | VAPOR DIFFUSION, SITTING DROP | 4.6 | 290 | 0.1 M ammonium acetate, 0.1 M sodium acetate, 24-30% PEG 4000; crystal obtained by streak-seeding and soaked with 90 mM of fragment 10 with the SMILES code CC(C)CCN1C(O)=NC2=C1C(=O)N(C)C(=O)N2C |