Crystal structure of mutant rabbit PRP 121-230 (S174N)

Experimental procedure
Experimental methodSINGLE WAVELENGTH
Source typeSYNCHROTRON
Source detailsCLSI BEAMLINE 08ID-1
Synchrotron siteCLSI
Beamline08ID-1
Temperature [K]100
Detector technologyCCD
Collection date2008-07-08
DetectorMARMOSAIC 300 mm CCD
Wavelength(s)0.9793
Spacegroup nameP 21 21 21
Unit cell lengths29.590, 86.250, 87.080
Unit cell angles90.00, 90.00, 90.00
Refinement procedure
Resolution61.280 - 1.500
R-factor0.14961
Rwork0.147
R-free0.19318
Structure solution methodMOLECULAR REPLACEMENT
Starting model (for MR)3o79
RMSD bond length0.016
RMSD bond angle1.532
Data reduction softwareXDS
Data scaling softwareXSCALE
Phasing softwarePHASER
Refinement softwareREFMAC (5.7.0029)
Data quality characteristics
 OverallOuter shell
Low resolution limit [Å]60.0001.600
High resolution limit [Å]1.5001.500
Rmerge0.1160.460
Number of reflections36582
<I/σ(I)>17.594.64
Completeness [%]99.899.9
Redundancy4.64.8
Crystallization Conditions
crystal IDmethodpHtemperaturedetails
1VAPOR DIFFUSION, HANGING DROP6.5298100mM SODIUM CACODYLATE PH 6.5, 3.0M NACL, 30% GLYCEROL (cryoprotectant), VAPOR DIFFUSION, HANGING DROP, temperature 298K