Experimental procedure
| Experimental method | SINGLE WAVELENGTH | 
| Source type | ROTATING ANODE | 
| Source details | RIGAKU RU200 | 
| Temperature [K] | 293 | 
| Detector technology | IMAGE PLATE | 
| Collection date | 1996-08-15 | 
| Detector | RIGAKU | 
| Spacegroup name | P 21 21 21 | 
| Unit cell lengths | 49.780, 76.760, 35.140 | 
| Unit cell angles | 90.00, 90.00, 90.00 | 
Refinement procedure
| Resolution | 8.000 - 2.200 | 
| R-factor | 0.19 * | 
| Rwork | 0.190 | 
| R-free | 0.27600 | 
| Structure solution method | MOLECULAR REPLACEMENT | 
| Starting model (for MR) | 1azp | 
| RMSD bond length | 0.008 * | 
| RMSD bond angle | 1.940 * | 
| Phasing software | X-PLOR | 
| Refinement software | X-PLOR (3.851) | 
Data quality characteristics
| Overall | Outer shell | |
| Low resolution limit [Å] | 8.000 * | 2.010 | 
| High resolution limit [Å] | 2.200 * | 2.200 * | 
| Rmerge | 0.630 | |
| Number of reflections | 5268 * | |
| Completeness [%] | 73.8 * | 60.9 * | 
| Redundancy | 2 | 
Crystallization Conditions
| crystal ID | method | pH | temperature | details | 
| 1 | Vapor diffusion, sitting drop * | 6.5 | pH 6.5, VAPOR DIFFUSION, HANGING DROP | 
Crystallization Reagents in Literatures
| ID | crystal ID | solution | reagent name | concentration (unit) | details | 
| 1 | 1 | drop | Sac7d | 1.3 (mM) | |
| 2 | 1 | drop | DNA duplex | 1.3 (mM) | |
| 3 | 1 | drop | Tris-HCl | 2.5 (mM) | |
| 4 | 1 | drop | PEG400 | 2 (%) | |
| 5 | 1 | reservoir | PEG400 | 15 (%) | 