9DYA
CHIP-TPR in complex with the Hsp70 tail
Experimental procedure
| Experimental method | SINGLE WAVELENGTH |
| Source type | SYNCHROTRON |
| Source details | ALS BEAMLINE 4.2.2 |
| Synchrotron site | ALS |
| Beamline | 4.2.2 |
| Temperature [K] | 100 |
| Detector technology | CCD |
| Collection date | 2014-05-05 |
| Detector | ADSC QUANTUM 315r |
| Wavelength(s) | 1.000000 |
| Spacegroup name | C 2 2 21 |
| Unit cell lengths | 46.899, 74.363, 77.634 |
| Unit cell angles | 90.00, 90.00, 90.00 |
Refinement procedure
| Resolution | 39.670 - 1.890 |
| R-factor | 0.1938 |
| Rwork | 0.190 |
| R-free | 0.23370 |
| Structure solution method | MOLECULAR REPLACEMENT |
| RMSD bond length | 0.010 |
| RMSD bond angle | 1.156 |
| Data reduction software | XDS |
| Data scaling software | XDS |
| Phasing software | PHASER |
| Refinement software | PHENIX (1.21rc1_5127) |
Data quality characteristics
| Overall | Outer shell | |
| Low resolution limit [Å] | 39.670 | 1.980 |
| High resolution limit [Å] | 1.890 | 1.890 |
| Rmerge | 0.170 | 1.014 |
| Rpim | 0.101 | 0.655 |
| Number of reflections | 20723 | 2406 |
| <I/σ(I)> | 7.05 | 0.99 |
| Completeness [%] | 98.9 | 91.46 |
| Redundancy | 3.8 | 3.2 |
| CC(1/2) | 0.988 | 0.442 |
Crystallization Conditions
| crystal ID | method | pH | temperature | details |
| 1 | VAPOR DIFFUSION, SITTING DROP | 8.5 | 298 | 0.2 M lithium sulfate, 0.1 M Tris-HCl, 30% (w/v) PEG 4000 |