9CR9
Crystal structure of MA6 Fab in complex with PfCSP repeat region peptide NPNA3
Experimental procedure
| Experimental method | SINGLE WAVELENGTH |
| Source type | SYNCHROTRON |
| Source details | APS BEAMLINE 19-ID |
| Synchrotron site | APS |
| Beamline | 19-ID |
| Temperature [K] | 100 |
| Detector technology | PIXEL |
| Collection date | 2019-06-22 |
| Detector | DECTRIS PILATUS3 X 6M |
| Wavelength(s) | 0.9795 |
| Spacegroup name | P 1 21 1 |
| Unit cell lengths | 46.600, 61.050, 152.999 |
| Unit cell angles | 90.00, 90.00, 90.00 |
Refinement procedure
| Resolution | 47.720 - 1.800 |
| R-factor | 0.1868 |
| Rwork | 0.185 |
| R-free | 0.21510 |
| Structure solution method | MOLECULAR REPLACEMENT |
| RMSD bond length | 0.008 |
| RMSD bond angle | 0.964 |
| Data reduction software | iMOSFLM |
| Data scaling software | Aimless |
| Phasing software | PHASER |
| Refinement software | PHENIX (1.20.1_4487) |
Data quality characteristics
| Overall | Outer shell | |
| Low resolution limit [Å] | 47.720 | 1.864 |
| High resolution limit [Å] | 1.800 | 1.800 |
| Rmerge | 0.077 | 0.433 |
| Rmeas | 0.109 | 0.613 |
| Rpim | 0.077 | 0.433 |
| Number of reflections | 74608 | 7426 |
| <I/σ(I)> | 5.93 | 2.14 |
| Completeness [%] | 93.3 | 93.07 |
| Redundancy | 1.8 | |
| CC(1/2) | 0.941 | 0.626 |
Crystallization Conditions
| crystal ID | method | pH | temperature | details |
| 1 | VAPOR DIFFUSION, SITTING DROP | 293 | 27% PEG3350, 3% MPD |