4OY7
Structure of cellulose active LPMO CelS2 (ScLPMO10C) in complex with Copper.
Experimental procedure
| Experimental method | SINGLE WAVELENGTH |
| Source type | SYNCHROTRON |
| Source details | BESSY BEAMLINE 14.1 |
| Synchrotron site | BESSY |
| Beamline | 14.1 |
| Temperature [K] | 100 |
| Detector technology | CCD |
| Collection date | 2012-11-27 |
| Detector | RAYONIX MX-225 |
| Wavelength(s) | 0.98 |
| Spacegroup name | P 21 21 21 |
| Unit cell lengths | 83.858, 122.856, 156.000 |
| Unit cell angles | 90.00, 90.00, 90.00 |
Refinement procedure
| Resolution | 47.900 - 1.500 |
| R-factor | 0.19517 |
| Rwork | 0.194 |
| R-free | 0.22238 |
| Structure solution method | MOLECULAR REPLACEMENT |
| RMSD bond length | 0.010 |
| RMSD bond angle | 1.385 |
| Refinement software | REFMAC (5.7.0032) |
Data quality characteristics
| Overall | Outer shell | |
| Low resolution limit [Å] | 47.900 | 1.580 |
| High resolution limit [Å] | 1.500 | 1.500 |
| Rmerge | 0.103 | 0.540 |
| Number of reflections | 254063 | |
| <I/σ(I)> | 5.9 | 1.7 |
| Completeness [%] | 99.1 | 94.2 |
| Redundancy | 3.9 | 2.7 |
Crystallization Conditions
| crystal ID | method | pH | temperature | details |
| 1 | VAPOR DIFFUSION, HANGING DROP | 4.5 | 293 | 9 % w/v PEG 10K, 0.1 M sodium citrate, 0.1 M calcium acetate, 5 % v/v glycerol |